Analysis of the compactibility of bituminous mixtures for reflective crack relief interlayers (RCRI)

Authors

DOI:

https://doi.org/10.24425/ace.2024.148907

Abstract

The physical properties determining the strength parameters of bituminous mixtures are strongly influenced by the processes of placement and compaction. The effectiveness of this process depends on the compactive effort and is directly related to the mixture temperature. This research focused on the assessment of compactibility of mixtures designed for reflective crack relief interlayers (RCRI) which, in most cases, are applied in thin layers. The materials analysed for compactibility in this research included AC – asphalt concrete, AC AF – asphalt concrete “anti-fatigue”, SMA – stone mastic asphalt and SMA-MA – stone mastic asphalt rich in bitumen mastic. The gyratory compactor method was used to determine the compaction slope K, the locking point LP and the compaction densification index CDI. All the tested mixtures were fine-graded, i.e., contained grains up to 8 mm in diameter, each mixed with a different type of bituminous binder. The values of CDI show a substantially greater input of energy required for compaction of high-polymer modified mixtures, as compared to mixtures of the same design, yet containing the 50/70 bitumen. Locking point analysis showed that SMA and SMA-MA mixtures attain 98% relative compaction before reaching the locking point at which the aggregate skeleton starts to resist further compaction. This is quite the opposite as with the AC and AC AF mixtures. Among the tested mixtures the best compaction behaviour was observed in the case of SMA-MA 8 50/70, and this over a wide range of working temperature (100–160 C) and pressures (150 kPa, 600 kPa). The design of the mixture SMA-MA as an anti-fatigue layer assumes an increase in the content of filler and binder, as compared to conventional SMA. This composition is bound to reduce the resistance to compaction, i.e., provide a better compaction behaviour as compared to a conventional SMA mixture.

References

[1] J.P. Mahoney, “Study of long-lasting pavements in Washington state”, Transportation Research Circular, no. 503, pp. 88–95, 2001. [Online]. Available: https://trid.trb.org/view/717438. [Accessed: 19 Sep. 2022].

[2] M. Nagórska, R. Nagorski, and K. Blazejowski, “Selected aspects of design lifespan of flexible pavement with anti-fatigue course”, Archives of Civil Engineering, vol. 61, no. 1, pp. 103–118, 2015, doi: 10.1515/ace-2015-0007.

[3] D.E. Newcomb, M. Buncher, and I.J. Huddleston, “Concepts of perpetual pavements”, Transportation Research Circular, no. 503, 2001. [Online]. Available: https://trid.trb.org/view/717432. [Accessed: 19 Sep. 2022].

[4] I. Ruttmar, A. Grajewska, and K. Pełczyńska, Perpetual pavement design and construction using anti-fatigue base layer on expressway S8 in Poland. Prague, 2016, doi: 10.14311/EE.2016.175.

[5] P. Radziszewski, J. Piłat, M. Sarnowski, J. Król and K.J. Kowalski, Nawierzchnie asfaltowe na obiektach mostowych. Warszawa: Oficyna Wydawnicza Politechniki Warszawskiej, 2016.

[6] W. Bańkowski and M. Gajewski, “Badania przyspieszone w skali rzeczywistej innowacyjnych nawierzchni drogowych”, Roads and Bridges – Drogi i Mosty, vol. 11, no. 2, pp. 89–121, 2012.

[7] B. Budziński and P. Mieczkowski, “Application of innovative SMA-MA mixtures on bridges”, Applied Sciences, vol. 10, no. 19, 2020, doi: 10.3390/app10196958.

[8] P. Mieczkowski, S. Majer, and B. Budziński, “Heavy maintenance of concrete paved roads using the regional roads No. 102 and No. 142 as an example”, Roads and Bridges – Drogi i Mosty, vol. 18, no. 1, pp. 25–38, 2019, doi: 10.7409/rabdim.019.002.

[9] P. Mieczkowski and B. Budzinski, “Influence of the type of HMA and free space content and the thermal conductivity coefficient λ”, IOP Conference Series: Materials Science and Engineering, vol. 603, no. 4, 2019, doi: 10.1088/1757-899X/603/4/042014.

[10] P. Mieczkowski, “The heat exchange in the edge area – the problem of hot mix asphalt compaction”, The Baltic Journal of Road and Bridge Engineering, vol. 10, no. 3, 2015, doi: 10.3846/bjrbe.2015.26.

[11] B.V. Kök, M. Yilmaz, and T. Alataş “Evaluation of the mechanical properties of field- and laboratory-compacted hot-mix asphalt”, Journal of Materials in Civil Engineering, vol. 26, no. 9, 2014, doi: 10.1061/(ASCE)MT.1943-5533.0000963.

[12] B. Dołżycki and J. Judycki, “Wpływ metod zagęszczania mieszanek mineralno-asfaltowych na wyniki badan ich cech mechanicznych”, Zeszyty Naukowe Politechniki Gdańskiej. Budownictwo Lądowe, no. 60, pp. 129–136, 2006.

[13] J.M. Gudimettla, L.A. Cooley, and E.R. Brown, “Workability of Hot-Mix Asphalt”, Transportation Research Board, vol. 1891, no. 1, pp. 229–237, 2004, doi: 10.3141/1891-27.

[14] A.E. Hunter, G.D. Airey, and A.C. Collop, “Aggregate orientation and segregation in laboratory-compacted asphalt samples”, Transportation Research Board, vol. 1891, no. 1, pp. 8–15, 2004, doi: 10.3141/1891-02.

[15] R. Miró, A. H. Martínez, F. E. Pérez-Jiménez, R. Botella, and A. Álvarez, “Effect of filler nature and content on the bituminous mastic behaviour under cyclic loads”, Construction Building Materials, vol. 132, pp. 33–42, 2017, doi: 10.1016/j.conbuildmat.2016.11.114.

[16] J. Pei, Y. Bi, J. Zhang, R. Li, and G. Liu, “Impacts of aggregate geometrical features on the rheological properties of asphalt mixtures during compaction and service stage”, Construction Building Materials, vol. 126, pp. 165–171, 2016, doi: 10.1016/j.conbuildmat.2016.09.033.

[17] A. Plewa, “Ocena wpływu wskaźnika zagęszczenia na moduł sztywności betonu asfaltowego”, Budownictwo i Inżynieria Środowiska, vol. 3, no. 3, pp. 133–139, 2012.

[18] M.R. Pouranian and J. E. Haddock, “Effect of aggregate gradation on asphalt mixture compaction parameters”, Journal of Materials in Civil Engineering, vol. 32, no. 9, 2020, doi: 10.1061/(ASCE)MT.1943-5533.0003315.

[19] H. Saedi, “Assessment of Compaction Temperatures on Hot Mix Asphalt (HMA) Properties”, International Journal of Civil and Geological Engineering, no. 6, pp. 159–163, 2012.

[20] B. Stefańczyk and P. Mieczkowski, Mieszanki mineralno-asfaltowe: wykonawstwo i badania. Warszawa: Wydawnictwa Komunikacji i Łączności, 2009.

[21] ASTM/D6925-15 Standard Test Method for Preparation and Determination of the Relative Density of Asphalt Mix Specimens by Means of the Superpave Gyratory Compactor. American Society for Testing and Materials.

[22] P. Tutka, M. Złotowska, K. Błazejowski, and R. Nagórski, “The influence of highly modified asphalt binder on pavement fatigue life prediction – selected problems”, Archives of Civil Engineering, vol. 67, no. 4, pp. 605–624, 2021, doi: 10.24425/ace.2021.138521.

[23] M. Kucińska, “Zagęszczanie próbek mieszanek mineralno-asfaltowych z wykorzystaniem prasy żyratorowej”, Drogownictwo, no. 7–8, pp. 236–240, 2013.

[24] F. Leiva and R. C.West, “Analysis of Hot-Mix Asphalt Lab Compactability Using Lab Compaction Parameters and Mix Characteristics”, Transportation Research Board, vol. 2057, no. 1, pp. 89–98, 2008, doi: 10.3141/2057-11.

[25] P. Li, J. Su, P. Gao, X. Wu, and J. Li, “Analysis of aggregate particle migration properties during compaction process of asphalt mixture”, Construction Building Materials, vol. 197, pp. 42–49, 2019, doi: 10.1016/j.conbuildmat.2018.11.164.

[26] P. Polaczyk, B. Huang, X. Shu, and H. Gong, “Investigation into Locking Point of Asphalt Mixtures Utilizing Superpave and Marshall Compactors”, Journal of Materials in Civil Engineering, vol. 31, no. 9, 2019, doi: 10.1061/(ASCE)MT.1943-5533.0002839.

[27] P. Polaczyk, Y. Ma, W. Hu, R. Xiao, X. Jiang, and B. Huang, “Effects of Mixture and Aggregate Type on Over-Compaction in Hot Mix Asphalt in Tennessee”, Transportation Research Board, vol. 2676, no. 4, pp. 448–460, 2022, doi: 10.1177/03611981211061558.

[28] EN 12697-10:2018-02 Bituminous mixtures – test method – Part10: Compatibility.

[29] K. Al-shamsi and L. Mohammad, “A Look at the Bailey Method and Locking Point Concept in Superpave Mixture Design”, Transportation Research Circular, E-C124, pp. 12–32, 2007.

[30] P. Polaczyk, B. Han, B. Huang, X. Jia, and X. Shu, “Evaluation of the hot mix asphalt compactability utilizing the impact compaction method”, Construction and Building Materials, vol. 187, pp. 131–137, 2018, doi: 10.1016/j.conbuildmat.2018.07.117.

[31] W.R. Vavrik and S.H. Carpenter, “Calculating Air Voids at Specified Number of Gyrations in Superpave Gyratory Compactor”, Transportation Research Board, vol. 1630, no. 1, pp. 117–125, 1998, doi: 10.3141/1630-14.

[32] Y. Du, P. Liu, J. Tian, J. Zhang, and Y. Zheng, “Preliminary Investigation of the Feasibility of Using a Superpave Gyratory Compactor to Design Cement-Treated Aggregate Mixture”, Applied Sciences, vol. 8, no. 6, 2018, doi: 10.3390/app8060946.

[33] A.F.F. Mahmoud and H. Bahia, Using gyratory compactor to measure mechanical stability of asphalt mixtures. Wisconsin Highway Research Program, Technical Report, Oct. 2004. [Online]. Available: http://digital.library.wisc.edu/1793/6907. [Accessed: 19 Sep. 2022].

Downloads

Published

2024-03-30

How to Cite

Merska, Oliwia, et al. “Analysis of the Compactibility of Bituminous Mixtures for Reflective Crack Relief Interlayers (RCRI)”. Archives of Civil Engineering, vol. 70, no. 1, Mar. 2024, pp. 201-17, doi:10.24425/ace.2024.148907.

Issue

Section

Articles

Similar Articles

<< < 5 6 7 8 9 10 11 12 13 14 > >> 

You may also start an advanced similarity search for this article.