Effect of Titanium Addition on Microstructure and Properties of Nitrogen-Alloyed High Chromium Cast Iron
DOI:
https://doi.org/10.24425/afe.2026.158031Abstract
This paper investigates the effect of titanium alloying on the eutectic transformation of high-chromium cast iron (HCCI) containing a significant amount of nitrogen (2.4% C, 30% Cr, 0.1% N). The study was conducted under industrial conditions in a Polish foundry, with titanium added to liquid HCCI as ferroalloy. Maximum Ti concentrations did not exceed 1.5%. The influence of titanium was assessed via characteristic points on crystallization curves recorded by thermal analysis, compared to the equilibrium phase diagram modeled by Thermo-Calc software. Microstructure was examined by XRD and SEM-EDS, revealing TiN precipitation. Abrasion resistance was evaluated using the Miller test. Titanium addition slightly lowered the eutectic transformation temperature and shifted crystallization from eutectic to hypereutectic of HCCI and reduced cumulative mass loss by 35% in the Miller abrasion test.
References
[1] Studnicki, A., Dojka, R., Gromczyk, M. & Kondracki, M. (2016). Influence of Titanium on crystallization and wear resistance of high chromium cast iron. Archives of Foundry Engineering. 16(1), 117-123. DOI: 10.1515/afe-2016-0014.
[2] Huang, Z.F., Xing, J.D., Zhi, X.H. & Gao, Y.M. (2014). Effect of Ti addition on morphology and size of primary M7C3 type carbide in hypereutectic high chromium cast iron. Materials Science and Technology. 27(1), 426-430. DOI: 10.1179/026708309X12601952777666.
[3] Dojka, M. & Stawarz, M. (2020) Bifilm defects in Ti-inoculated chromium white cast iron. Materials. 13(14), 1-19. DOI: 10.3390/ma13143124.
[4] Zhi, X., Xing, J., Fu, H. & Gao, Y. (2008). Effect of titanium on the as-cast microstructure of hypereutectic high chromium cast iron. Materials Characterization. 59(9), 1221-1226. DOI: 10.1016/j.matchar.2007.10.010.
[5] Wu, X., Xing, J., Fu, H. & Zhi, X. (2007). Effect of titanium on the morphology of primary M7C3 carbides in hypereutectic high chromium white iron. Materials Science and Engineering A. 457(1-2), 180-105. DOI: 10.1016/j.msea.2006.12.006.
[6] Kim, W. Y., Jo, J. O., Chung, T. I., Kim, D. S., & Pak, J. J. (2007). Thermodynamics of titanium, nitrogen and TiN formation in liquid iron. ISIJ International. 47(8), 1082-1089. https://doi.org/10.2355/isijinternational.47.1082.
[7] Pak, J. J., Jeong, Y. S., Hong, I. K., Cha, W. Y., Kim, D. S., & Lee, Y. Y. (2005). Thermodynamics of TiN formation in Fe-Cr melts. ISIJ international, 45(8), 1106-1111.
[8] Ding, H., Liu, S., Zhang, H., Guo, J. (2015). Improving impact toughness of a high chromium cast iron regarding joint additive of nitrogen and titanium. Materials and Design. 90, 958-968. http://dx.doi.org/10.1016/j.matdes.2015.11.055.
[9] Bramfit, B.L. (1970). The effect of carbide and nitride additions on the heterogeneous nucleation behavior of liquid iron. Metallurgical Transactions. 1, 1987-1995. https://doi.org/10.1007/BF02642799.
[10] Ovcharenko, G., Nikonova, R.M., Tereshkina, S.A. & Lubnin, A.N. (2023) Influence of nitrogen on chromium cast iron structure and properties. Metallurgist. 67(3-4), 452-461. DOI:10.1007/s11015-023-01531-2.
[11] Shen, L.R., Wang, K., Tie , J., Tong, H.H., Chen, Q.C., Tang, D.L., Fu, R.K.Y. & Chu P.K. (2005). Modification of high-chromium cast iron alloy by N and Ti ion implantation. Surface & Coatings Technology. 196, 349-352. DOI: 10.1016/j.surfcoat.2004.08.165.
[12] Dojka, M., Kondracki, M., Studnicki, A. & Dojka, R. (2018). Crystallization process of high chromium cast iron with the addition of Ti and Sr. Archives of Foundry Engineering. 18(2), 57-64. DOI: 10.24425/122503.
[13] Dojka, M., Dojka, R., Stawarz, M. & Studnicki, A. (2019). Influence of Ti and REE on Primary Crystallization and Wear Resistance of Chromium Cast Iron. Journal of Materials Engineering and Performance. 28, 4002-4011. https://doi.org/10.1007/s11665-019-04088-x.
[14] Bedolla-Jacuinde, A., Correa, R., Quezada, J.G. & Maldonado, C. (2005). Effect of titanium on the as-cast microstructure of a 16%chromium white iron. Materials Science and Engineering A. 398(1-2), 297-308. DOI: 10.1016/j.msea.2005.03.072.
[15] Chunga, R.J., Tanga, X., Li, D.Y., Hinckley, B. & Dolman, K. (2009). Effects of titanium addition on microstructure and wear resistance of hypereutectic high chromium cast iron Fe–25wt.%Cr–4wt.%C. Wear. 267(1-4), 356-361. DOI: 10.1016/j.wear.2008.12.061.
[16] Liu, T., Sun, J., Xiao, Z., He, J. Shi, W. & Cui, C. (2023). Effect of multi-element microalloying on the structure and properties of high chromium cast iron. Materials. 16(9), 3292, 1-12. https://doi.org/10.3390/ma16093292.
[17] Gong, L., Fu, H., Yang, P., Ji, X., Yin, W. & Lin, J. (2023). Refinement of primary carbides and improvement of wear resistance of hypereutectic high chromium cast iron after modification. Journal of Materials Research and Technology. 24, 5724-5742. https://doi.org/10.1016/j.jmrt.2023.04.176.
[18] Wang, J., Xing, X., Zhou, Y., Qi, X. & Yang, Q. (2010). Refining effect of nitrogen on M7C3 carbides in hypereutectic Fe–25Cr–4C–0.5Ti–0.5Nb hardface coatings. Materials Science and Technology. 35(9), 1114-1122. DOI:10.1080/02670836.2019.1613060.
[19] Jo, J., Kim, W., Lee, C. & Pak, J. (2010). Thermodynamic Interaction between Chromium and Titanium in Liquid Fe–Cr Alloys Containing 30 mass% Cr. ISIJ International. 50(10), 1373-1379. https://doi.org/10.2355/isijinternational.50.1373.
[20] Pierson, H.O. (1996). Handbook of Refractory Carbides and Nitrides: Properties, Characteristics, Processing and Applications. Westwood, NJ: Noyes Publications. https://doi.org/10.1016/B978-081551392-6.50001-5.
[21] Wiengmoon, A., Chairuangsri, T., Brown, A., Brydson, R. Edmonds, D.V. & Pearce J.T.H. (2005). Microstructural and crystallographical study of carbides in 30wt.%Cr cast irons. Acta Materialia. 53(15), 4143-4154. DOI: 10.1016/j.actamat.2005.05.019.
[22] Liu, Q., Zhang, H., Wang, Q., Zhou, X., Jönsson, P.G. & Nakajima, K. (2012). Effect of cooling rate and Ti addition on the microstructure and mechanical properties in as-cast condition of hypereutectic high chromium cast irons. ISIJ International. 52(12), 2210-2219, https://doi.org/10.2355/isijinternational.52.2210.
[23] Tabrett, C.P., Sare, I.R. & Ghomashchi, M.R. (1996). Microstructure-property relationships in high chromium white iron alloys. International Materials Reviews. 41(2), 59-82. https://doi.org/10.1179/imr.1996.41.2.59.
[24] Zum Gahr, K.H. & Eldis, G.T. (1980). Abrasive wear of white cast irons. Wear. 64(1), 175-194. DOI: 10.1016/0043-1648(80)90101-5.
[25] Doğan, Ö.N. & Hawk J.A. (1995). Effect of carbide orientation on abrasion of high Cr white cast iron. Wear. 189(1-2), 136-142. DOI: 10.1016/0043-1648(95)06682-9.
[26] Doğan, Ö.N., Hawk, J.A. & Laird G. (1997). Solidification structure and abrasion resistance of high chromium white irons. Metallurgical and Materials Transactions A. 28, 1315-1328. https://doi.org/10.1007/s11661-997-0267-3.
Downloads
Published
How to Cite
Issue
Section
License
Copyright (c) 2026 Archives of Foundry Engineering

This work is licensed under a Creative Commons Attribution 4.0 International License.